Fine ceramics (advanced ceramics, advanced technical ceramics). Test method for GaN crystal surface defects. Method for determining etch pit density | Status: Current
description
1 Scope
This document describes a method for determining the etch pit density, which is used to detect dislocations and processing-introduced defects that occur on single-crystal GaN substrates or single-crystal GaN films.
It is applicable to the defects specified in ISO 5618‑1 from among the defects exposed on the surface of the following types of GaN substrates or films: single-crystal GaN substrate; single-crystal GaN film formed by homoepitaxial growth on a single-crystal GaN substrate; or single-crystal GaN film formed by heteroepitaxial growth on a single-crystal Al2O3, SiC, or Si substrate.
It is applicable to defects with an etch pit density of ≤ 7 × 107 cm-2.
Details
Publisher
BS
File size
2.92 MB
Pages
34
Format
PDF
Publication date
2024-05-07
ISBN-13
978-0-539-22479-5
ISBN-13 plain
9780539224795
ISBN-10
0539224795